Mechanical Properties Metric English Comments
Tensile Strength 517 - 703 MPa
75000 - 102000 psi
Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze
Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Ext..