Polymer Property : Tensile Strength = 6500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 44.8 MPa
6500 psi
ASTM D638
Quadrant EPP TIVAR® Oil Filled UHMW-PE FDA/USDA Oil-Filled UHMW-PE (ASTM Product Data Sheet)
Tensile Strength 44.8 MPa
6500 psi
ASTM D638
Teknor Apex Chemlon® 275H Nylon 6, Copolymer, Impact Modified
Notes: Very high impact and elongation, low flexural modulus material for tubing and wire jacketing applications requiring a soft, flexible product; FMVSS Flammability: Passes, FMVSS 302Processing M..
Tensile Strength 44.8 MPa
6500 psi
ASTM D638
Techmer ES Luriblend® ABS TX15
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(15%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc.
Tensile Strength 44.8 MPa
6500 psi
ASTM D638, ASTM D1708
ScanTube ETFE Tubing
Information provided by ScanTube, Inc.
Tensile Strength >= 44.8 MPa
>= 6500 psi
Master Bond EP38 Low Viscosity, Fast Curing, Two Component Epoxy
Master Bond Polymer System EP38 is a fast curing, low viscosity, optically clear two component epoxy system for high performance coating, bonding and sealing. EP38 has a unique balance of favorable ..
Tensile Strength >= 44.8 MPa
>= 6500 psi
Master Bond Supreme 3HTND-2GT One Part, Toughened, Fast Curing Glob Top Adhesive
Master Bond Polymer System Supreme 3HTND-2GT is a fast curing, toughened one component high performance epoxy adhesive/sealant which meets the growing need for precise positioning and bonding of mic..
Tensile Strength 44.8 MPa
6500 psi
ASTM D412
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane
Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo..
Tensile Strength 44.8 MPa
6500 psi
ASTM D638
Ecomass® 1700CO93 Copper Powder Filled Polyamide, Injection Molding
High Specific Gravity, Copper Powder Filled Polyamide (PA), Rigid, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInform..
Tensile Strength 44.8 MPa
6500 psi
IPC TM-650 2.4.18.3
Arlon 85NT Polyimide Nonwoven Aramid Laminate and Prepreg
85NT is a pure polyimide laminate and prepreg system (Tg = 250°C), reinforced with a non-woven aramid substrate. This system combines the high-reliability features of polyimide (improved PTH relia..
Tensile Strength 44.8 MPa
6500 psi
ASTM D638
Americas Styrenics MC3650 High Heat Crystal Polystyrene
Product CharacteristicsImproved cycle times in hard to fill partsExcellent clarity with slight blue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsHousewaresConsumer..
Tensile Strength 44.8 MPa
6500 psi
IPC TM-650 2.4.18.3
Arlon 51N Lead-Free Compatible Epoxy Low-Flow
51N is a non-DICY multifunctional epoxy low-flow prepreg system designed to provide high reliability through lead-free solder operations. The high decomposition temperature and high thermal stabili..
Tensile Strength 44.8 MPa
6500 psi
ASTM D638
Aaron Industries AAROPRENE® AE PC/ABS 7000-2 PC/ABS Engineered Resin
Melt flow index may be specified.
Tensile Strength 44.8 MPa
6500 psi
ASTM D638
Aaron Industries AAROPRENE® GFPP 2020 Glass Filled Polypropylene
AAROPRENE® GFPP 2000 Series Glass Reinforced CompoundsMelt flow index may be specified. Color may be specified.