Polymer Property : Tensile Strength = 64.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 64.0 MPa
9280 psi
ISO 527-2
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin
Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim
Tensile Strength 64.0 MPa
9280 psi
ISO 527-2
NOVA Chemicals Dylark® 510XT Glass Reinforced Engineering Resin
Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri..
Tensile Strength 64.0 MPa
9280 psi
ASTM D638
Kolon KOCETAL® K900 Standard Grade Acetal Resin
Very low viscosity grade. Applications: Thin and large products.Information provided by API-Kolon.
Tensile Strength 64.0 MPa
9280 psi
ASTM D638
Kolon KOCETAL® VT702 Anti-Static Grade Acetal Resin
Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon.
Tensile Strength 64.0 MPa
9280 psi
Volume Resistivity 3 [log(ohm-cm)]
TIMCAL ENSACO™ 250G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..