Tensile Strength >= 36.3 MPa
>= 5260 psi
ASTM D 638
Karina E 813-10/369-BY-ERYB White PVC Compound
Rigid PVC compound recommended to extrude general profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength 36.3 MPa
5260 psi
50 mm/min; ISO 527-1,-2
Gromax BTE65-DN001N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Strength 36.3 MPa
5260 psi
ASTM D638M
Asia Technology Pioneers CAP 101 PP Nanocomposite
Description: CAP101 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim..