Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 36.3 MPa | >= 5260 psi | ASTM D 638 |
Karina E 813-10/369-BY-ERYB White PVC Compound Rigid PVC compound recommended to extrude general profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 36.3 MPa | 5260 psi | 50 mm/min; ISO 527-1,-2 |
Gromax BTE65-DN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 36.3 MPa | 5260 psi | ASTM D638M |
Asia Technology Pioneers CAP 101 PP Nanocomposite Description: CAP101 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |