Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 345 MPa @Thickness 1.02 - 38.1 mm |
50000 psi @Thickness 0.0400 - 1.50 in |
Rolled Plate |
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining.. |
|||
Tensile Strength | 345 MPa @Thickness 38.13 - 76.2 mm |
50000 psi @Thickness 1.501 - 3.00 in |
Rolled Plate |
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining.. |