Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 345 MPa

@Thickness 1.02 - 38.1 mm
50000 psi

@Thickness 0.0400 - 1.50 in
Rolled Plate
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining..
Tensile Strength 345 MPa

@Thickness 38.13 - 76.2 mm
50000 psi

@Thickness 1.501 - 3.00 in
Rolled Plate
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining..