Polymer Property : Tensile Strength = 485 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 3.34 MPa
485 psi
Silicone Property; ASTM D412
Arlon R36580N008 0.008" ((0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat..
Tensile Strength 3.34 MPa
485 psi
Silicone Property; ASTM D412
Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat..