Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 3.34 MPa | 485 psi | Silicone Property; ASTM D412 |
Arlon R36580N008 0.008" ((0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat.. |
|||
Tensile Strength | 3.34 MPa | 485 psi | Silicone Property; ASTM D412 |
Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat.. |