GRECO ISOTHANE 3055D Polyether TPU Resin

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer GRECO
Trade Name ISOTHANE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GRECO ISOTHANE 3055D Polyether TPU Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These products can be injection molded, blow molded, and extruded.Information provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength 44.0 MPa
6380 psi
ASTM D412
Tensile Strength, Yield 13.0 MPa

@Strain 50.0 %
1890 psi

@Strain 50.0 %
ASTM D412
17.0 MPa

@Strain 100 %
2470 psi

@Strain 100 %
ASTM D412
31.0 MPa

@Strain 300 %
4500 psi

@Strain 300 %
ASTM D412
Elongation at Break 430 %
430 %
ASTM D412
Tear Strength 850 kN/m
4850 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 70
70
ASTM D1044(Taber) H-22
Compression Set 25 %

@Temperature 23.0 °C,
Time 79200 sec
25 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
35 %

@Temperature 70.0 °C,
Time 79200 sec
35 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395