Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 38.6 MPa | 5600 psi | ASTM D-638 |
Plaskolite Optix® CA - 2000 HF-4-2 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Tensile Strength | 38.6 MPa | 5600 psi | ASTM D-638 |
Plaskolite Optix® CA - 2000 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Tensile Strength | 38.6 MPa | 5600 psi | ASTM D638 |
Quadrant EPP TIVAR® Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet) |
|||
Tensile Strength | >= 38.6 MPa | >= 5600 psi | ASTM D 638 |
Karina E 836-10/185-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 38.6 MPa | >= 5600 psi | ASTM D 638 |
Karina E 854-10/150-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 38.6 MPa | >= 5600 psi | ASTM D 638 |
Karina E 854-10/185-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 38.6 MPa | >= 5600 psi | ASTM D 638 |
Karina E 855-10/150-ERYB-PO White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 38.6 MPa | 5600 psi | 2 in/min; ASTM D638 |
Braskem FT120WV Homopolymer Polypropylene Description: Antistatic, nucleated, good mold release.Applications: Suggested uses include cosmetic packaging, disposable cutlery, closures, overcaps.Process: Injection Molding.This resin meets the .. |
|||
Tensile Strength | 38.6 MPa | 5600 psi | 2 in/min; ASTM D638 |
Braskem FT200WV Homopolymer Polypropylene Description: Good mold release, nucleated, excellent rigidity and hardness.Applications: Suggested uses include housewares, caps and closures, fast-cycle injection molding.Process: Injection Molding.. |
|||
Tensile Strength | 38.6 MPa | 5600 psi | ASTM D-638 |
Plaskolite West Optix® CA - 2000 HF-4-2 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Tensile Strength | 38.6 MPa | 5600 psi | ASTM D-638 |
Plaskolite West Optix® CA - 2000 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Tensile Strength | 38.6 MPa | 5600 psi | |
Henkel Hysol EA 9330 Paste Adhesive System Easy mix adhesive with high peel strength and excellent environmental durability.Applications: Structural Repair Composite Bonding |