Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 23.4 MPa
3390 psi
Typical properties of film cast from toluene solution; ASTM D412
Kraton® G1657 M (SEBS) Linear Triblock Copolymer
Description: Kraton G1657 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form id..
Tensile Strength 23.4 MPa
3390 psi
ASTM D638
KYDEX® 6200 LTR Thermoforming Sheet for Mass Transit Applications
Features:Specifically designed for mass transit industriesCompliant with SMP800CMeets flamespread and smoke density requirements for mass transitExcellent formability and fabrication qualityGood def..
Tensile Strength 23.4 MPa
3390 psi
ASTM D4894
Saint-Gobain Fluoroloy® A15 High Performance Seal Material
Improved sealing at low pressure; Can be abrasive running against soft metals Information provided by Saint-Gobain Performance Plastics.
Tensile Strength 23.4 MPa
3390 psi
Conductive CR Conveyor Belt Cover Compound
TIMCAL ENSACO™ 250G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
Tensile Strength 23.4 MPa
3390 psi
ASTM D412
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane
Features: Very high tensile strength, excellent low temperature flexibility, and superior abrasion and cut resistanceUses: Extrusion – Wire and cable, Hose and tube & General purposeAvailable in Am..