Saint-Gobain Fluoroloy® A15 High Performance Seal Material

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Fluoroloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Fluoroloy® A15 High Performance Seal Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Improved sealing at low pressure; Can be abrasive running against soft metals Information provided by Saint-Gobain Performance Plastics.
Physical Properties Metric English Comments
Density 2.23 g/cc
0.0806 lb/in³
ASTM D792
Deformation 8.5 %

@Time 86400 sec
8.5 %

@Time 24.0 hour
13.8 MPa (2000 psi) load; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ASTM D2240
Tensile Strength 23.4 MPa
3390 psi
ASTM D4894
Elongation at Break 230 %
230 %
ASTM D4894
Tensile Modulus 0.441 GPa
64.0 ksi
ASTM D4894
Compressive Yield Strength 13.1 MPa

@Strain 1.00 %
1900 psi

@Strain 1.00 %
ASTM D695
Compressive Modulus 0.827 GPa
120 ksi
ASTM D695
Coefficient of Friction 0.090
0.090
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 129 µm/m-°C

@Temperature 26.0 - 200 °C
71.7 µin/in-°F

@Temperature 78.8 - 392 °F
Mold Direction; ASTM D696
CTE, linear, Transverse to Flow 93.5 µm/m-°C

@Temperature 26.0 - 200 °C
51.9 µin/in-°F

@Temperature 78.8 - 392 °F
ASTM D696
Maximum Service Temperature, Air 316 °C
601 °F
Minimum Service Temperature, Air -268 °C
-450 °F
Descriptive Properties Value Comments
Color Dark Gray