Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 23.4 MPa | 3400 psi | ASTM D638 |
Quadrant EPP Proteus® PP Natural Co-Polymer Polypropylene (ASTM Product Data Sheet) |
|||
Tensile Strength | 23.4 MPa | 3400 psi | Typical |
Garlock 135 Natural Sheet Rubber Garlock Natural Rubber Sheet is manufactured from Food and Drug Administration-approved ingredients. It is a superior, long-life sheet designed specifically for general gasketing, countertops and sk.. |
|||
Tensile Strength | 23.4 MPa | 3390 psi | Typical properties of film cast from toluene solution; ASTM D412 |
Kraton® G1657 M (SEBS) Linear Triblock Copolymer Description: Kraton G1657 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form id.. |
|||
Tensile Strength | 23.4 MPa | 3390 psi | ASTM D638 |
KYDEX® 6200 LTR Thermoforming Sheet for Mass Transit Applications Features:Specifically designed for mass transit industriesCompliant with SMP800CMeets flamespread and smoke density requirements for mass transitExcellent formability and fabrication qualityGood def.. |
|||
Tensile Strength | 23.4 MPa | 3390 psi | ASTM D4894 |
Saint-Gobain Fluoroloy® A15 High Performance Seal Material Improved sealing at low pressure; Can be abrasive running against soft metals
Information provided by Saint-Gobain Performance Plastics. |
|||
Tensile Strength | 23.4 MPa | 3390 psi | Conductive CR Conveyor Belt Cover Compound |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Tensile Strength | 23.4 MPa | 3390 psi | ASTM D412 |
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane Features: Very high tensile strength, excellent low temperature flexibility, and superior abrasion and cut resistanceUses: Extrusion – Wire and cable, Hose and tube & General purposeAvailable in Am.. |
|||
Tensile Strength | 23.4 MPa | 3400 psi | Cross; IPC TM-650 2.4.18.3 |
Arlon CLTE-XT High Precision Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
Tensile Strength | 23.4 MPa | 3400 psi | |
AlphaGary Garaflex™ E 50-10 B Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable90°C rated non-migrating jacket compound for Mil C 17G |
|||
Tensile Strength | 23.4 MPa | 3400 psi | |
AlphaGary PVC FM1R Polyvinyl Chloride Thermoplastic Resistant to UV, moisture and mildew for high speed extrusion of coated yarn for outdoors furniture, wire fence coating and automotive harness cable coating |