Arlon R36386C035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R36386C035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber (Ferromagnetic Filler) Substrate: Style 7628 Fiberglass This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
Side 1, Silicone Property; Arlon SQA-TMS-024
3.80 g/cc
0.137 lb/in³
Side 2, Silicone Property; Arlon SQA-TMS-024
Thickness 127 microns
5.00 mil
Side 1; Arlon SQA-TMS-003
127 microns
5.00 mil
Interleave
203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
559 microns
22.0 mil
Side 2; Arlon SQA-TMS-003
889 microns
35.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 37
37
Side 1, Silicone Property; ASTM D2240
70
70
Side 2, Silicone Property; ASTM D2240
Tensile Strength 2.07 MPa
300 psi
Side 2, Silicone Property; ASTM D412
6.21 MPa
900 psi
Side 1, Silicone Property; ASTM D412
Elongation at Break 110 %
110 %
Side 2, Silicone Property; ASTM D412
625 %
625 %
Side 1, Silicone Property; ASTM D412
Peel Strength 0.877 kN/m
5.00 pli
Bond Strength (S2 to S2); ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 9.84 kV/mm
250 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 80.5
Arlon SQA-TMS-025