Polymer Property : Tensile Strength = 27600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 190 MPa
27600 psi
RT; ASTM D638
Rogers Corporation XT/duroid™ 8100 0.004" Woven Glass Reinforced Thermoplastic Circuit Material
XT/duroid™ 8100 woven glass reinforced thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 81..
Tensile Strength 190 - 200 MPa
27600 - 29000 psi
ASTM D882-80
Isoflon Polyester film
Polyethylene terephthalate film is a flexible film with high mechanical resistance. An excellent insulator, it preserves all its properties in a wide range of temperatures (-70°C to +150°C). ..
Tensile Strength 190 MPa
27600 psi
ASTM D638
Kuraray Genestarâ„¢ GT2330 Nylon, 33% Glass Filled
Toughness V-0 Grade. It is well suited for components requiring a high strength in pin fitting process, due to high ductility properties.
Tensile Strength 190 MPa
27600 psi
5 mm/min; ISO 527-1
Sax Polymers SAXAMID 126F6 Nylon 6, 30% Glass Fiber
SAXAMID 126F6 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Other properties are ..
Tensile Strength 190 MPa
27600 psi
dry; ISO 527
Ter Hell Plastic Terez® PA 6.6 7510 GF 50 Polyamide 66, 50% Glass Fiber
Description: PA66 with medium viscosity, 50% glass fiber reinforced.Application: For molding parts with very high stiffness at good thermal stability.Information provided by Ter Hell Plastic GMBH...
Tensile Strength 190 MPa
27600 psi
ISO 527
Azoty Tarnow™ Tarnamid® T-27 CF30 Polyamide 6 30% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Tensile Strength 190 MPa
27600 psi
ISO 527
Azoty Tarnow™ Tarnamid® T-27 CF40 Polyamide 6 40% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Tensile Strength >= 190 MPa

@Temperature 1530 °C
>= 27600 psi

@Temperature 2780 °F
Zircar Ceramics MOSI2 Molybdenum Disilicide Heating Element
ZIRCAR Molybdenum Disilicide Heating Element Type MOSI2 is an electric element principally containing molybdenum disilicide for use in industrial and laboratory furnaces. Elements fabricated of thi..