Mechanical Properties Metric English Comments
Tensile Strength 179 MPa
26000 psi
ASTM D638
Quantum Composites HTC-9593 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite
HTC-9593 (127-51-5) is a 3K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristics..
Tensile Strength 179 MPa
26000 psi
ASTM D638
Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA), 25% GlassCarbon Fiber
Amodel® A-1625 HS is a 25% carbon and glass-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material..
Tensile Strength 179 MPa
26000 psi
ASTM D638
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even..
Tensile Strength 179 MPa
26000 psi
ASTM D638
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
Tensile Strength 179 MPa
26000 psi
ASTM D638
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi..
Tensile Strength 179 MPa
26000 psi
ASTM D638
Solvay Specialty Polymers Ryton® R-4-232NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-232NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations..
Tensile Strength 179 MPa
26000 psi
Machine; ASTM D882
Arlon CuClad 250 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 250 uses a higher fiberglass/PTFE ratio to provide mechanical properties approaching those of conventional substrates. Better dimensional stability and lower thermal expansion in all directi..
Tensile Strength 179 MPa
26000 psi
ASTM D638
Aaron Industries AAROPRENE® GFN 6633 Glass Filled Nylon 6/6
AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified.
Tensile Strength 179 MPa

@Temperature 260 °C
26000 psi

@Temperature 500 °F
Typical
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy
Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual ..
Tensile Strength 179 MPa
26000 psi
ASTM D638
Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1625 HS is a 25% carbon and glass-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material is ..