Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), Carbon Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel A-1625 HS is a 25% carbon and glass-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material is well suited for fuel systems applications requiring low permeation, low swell, and high thermal resistance. It can also be used for components of electrical/electronic systems requiring high strength and stiffness, as well as static charge dissipation. Amodel A-1625 HS provides low moisture absorption, excellent dimensional stability and has creep resistance superior to other electrostatic dissipative materials. - Black: A-1625 HS BK 324Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183/A
Filler Content 25 %
25 %
GlassCarbon Fiber Reinforcement
Water Absorption 0.25 %

@Temperature 23.0 °C,
Time 86400 sec
0.25 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength 179 MPa
26000 psi
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ISO 527-2
Tensile Modulus 13.0 GPa
1890 ksi
ISO 527-2
Flexural Strength 275 MPa
39900 psi
ISO 178
Flexural Modulus 10.9 GPa
1580 ksi
ISO 178
Izod Impact, Notched (ISO) 9.20 kJ/m²
4.38 ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 285 °C
545 °F
Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 275 °C
527 °F
Unannealed; ISO 75-2/A
Electrical Properties Metric English Comments
Volume Resistivity 2400 ohm-cm
2400 ohm-cm
50V; SAE J1645
Processing Properties Metric English Comments
Rear Barrel Temperature 310 °C
590 °F
Front Barrel Temperature 320 °C
608 °F
Melt Temperature 320 - 330 °C
608 - 626 °F
Mold Temperature 135 °C
275 °F
Drying Temperature 120 °C
248 °F
Dry Time 4.00 hour
4.00 hour
Moisture Content 0.060 %
0.060 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Appearance Black
Automotive Specifications ASTM D4000 PPA0110 G12 KB140 LB001 PA049 YA225 ZE01 ZK02 Color: BK-324 Black
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Good Chemical Resistance
Good Creep Resistance
Good Dimensional Stability
Good Stiffness
High Heat Resistance
High Stiffness
High Temperature Strength
Low Moisture Absorption
Forms Pellets
Generic PPA
Processing Method Injection Molding
Uses Automotive Applications
Automotive Electronics
Automotive Under the Hood
Connectors
Electrical/Electronic Applications
Fuel Lines
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved