Mechanical Properties Metric English Comments
Tensile Strength 26.5 MPa
3840 psi
ASTM D412
S&E Specialty Polymers GA-1046CTLF PVC
Application: Lead free 105° C tri-rated semi-rigid insulation compound suitable for UL style 1061, CSA-SRPVC, MIL-I-16878.Information provided by S&E Specialty Polymers
Tensile Strength 26.5 MPa
3840 psi
ASTM D638
Shinkong Synthetic Fibers Shinite® PP4220 PP, High Impact, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Tensile Strength 26.5 MPa
3840 psi
ASTM D638
Shinkong Synthetic Fibers Shinite® PP4220 PP, High Impact, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Tensile Strength 26.5 MPa
3850 psi
ASTM D638
Ecomass® 1005ZD96 Tungsten Powder Filled Co-Polyamide, Injection Molding Grade
High Specific Gravity, Tungsten Powder Filled Co-Polyamide (COPA), Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing ..
Tensile Strength 26.5 MPa
3850 psi
ASTM D638
Aaron Industries AAROPRENE® CFIPP 2020 High Impact Calcium Carbonate Filled Polypropylene
AAROPRENE® CFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.