Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 26.5 MPa | 3850 psi | ASTM D638 |
Ecomass® 1005ZD96 Tungsten Powder Filled Co-Polyamide, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Co-Polyamide (COPA), Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing .. |
|||
Tensile Strength | 26.5 MPa | 3850 psi | ASTM D638 |
Aaron Industries AAROPRENE® CFIPP 2020 High Impact Calcium Carbonate Filled Polypropylene AAROPRENE® CFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |