Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1670 MPa | 242000 psi | 50 HRC |
Schmolz + Bickenbach Thermodur® 2365 EFS Extra Fine Structure - Hot Work Die Steel Description: Thermodur® 2365 is an Extra Fine Structure (EFS) hot work tool steel developed for good high temperature strength and tempering resistance and Supplied in the annealed conditionChara.. |
|||
Tensile Strength | 1670 MPa @Treatment Temp. 200 °C |
242000 psi @Treatment Temp. 392 °F |
50 HRC |
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel Description: Cryodur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared t.. |
|||
Tensile Strength | 1670 MPa @Treatment Temp. 200 °C |
242000 psi @Treatment Temp. 392 °F |
50 HRC |
Schmolz + Bickenbach Formadur® 2311 Plastic Mold Steel Description: Formadur® 2311 is a pre-hardened plastic mold steelCharacteristics: Good texturing compared to Formadur®2312 and Good polishability compared to Formadur® 231Applications: Injection m.. |
|||
Tensile Strength | 1670 MPa @Treatment Temp. 200 °C |
242000 psi @Treatment Temp. 392 °F |
50 HRC |
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel Description: Formadur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared .. |
|||
Tensile Strength | 1670 MPa | 242000 psi | 50 HRC |
Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel Description: THERMODUR 2344 is a single melt Extra Fine Structure (EFS) hot work die steel; and Supplied in the annealed conditionCharacteristics: Good toughness; Good resistance to thermal shock a.. |