Tensile Strength 1670 MPa
242000 psi
50 HRC
Schmolz + Bickenbach Thermodur® 2365 EFS Extra Fine Structure - Hot Work Die Steel
Description: Thermodur® 2365 is an Extra Fine Structure (EFS) hot work tool steel developed for good high temperature strength and tempering resistance and Supplied in the annealed conditionChara..
Tensile Strength 1670 MPa

@Treatment Temp. 200 °C
242000 psi

@Treatment Temp. 392 °F
50 HRC
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel
Description: Cryodur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared t..
Tensile Strength 1670 MPa

@Treatment Temp. 200 °C
242000 psi

@Treatment Temp. 392 °F
50 HRC
Schmolz + Bickenbach Formadur® 2311 Plastic Mold Steel
Description: Formadur® 2311 is a pre-hardened plastic mold steelCharacteristics: Good texturing compared to Formadur®2312 and Good polishability compared to Formadur® 231Applications: Injection m..
Tensile Strength 1670 MPa

@Treatment Temp. 200 °C
242000 psi

@Treatment Temp. 392 °F
50 HRC
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel
Description: Formadur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared ..
Tensile Strength 1670 MPa
242000 psi
50 HRC
Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel
Description: THERMODUR 2344 is a single melt Extra Fine Structure (EFS) hot work die steel; and Supplied in the annealed conditionCharacteristics: Good toughness; Good resistance to thermal shock a..