Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 15.4 MPa | >= 2240 psi | ASTM D412 Method A |
Seals Eastern 5794 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |