Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 15.4 MPa | 2230 psi | ISO 37 |
Multibase TPSiV® 4200-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Tensile Strength | >= 15.4 MPa | >= 2240 psi | ASTM D412 Method A |
Seals Eastern 5794 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |