Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 2.50 MPa @Strain 200 % |
363 psi @Strain 200 % |
ISO 527 |
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Tensile Strength | 2.50 MPa | 363 psi | |
Shin-Etsu Silicones KE-3479 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 2.50 MPa | 363 psi | |
Shin-Etsu Silicones KE-347T Silicone, RTV Coating Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 2.50 MPa | 363 psi | |
Shin-Etsu Silicones KE-3490 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 2.50 MPa | 363 psi | |
Shin-Etsu Silicones KE-3490 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 2.50 MPa | 363 psi | |
Shin-Etsu Silicones KE-3494 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 2.50 MPa @Strain 20.0 % |
363 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan 1185 A W TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 2.50 MPa @Strain 100 % |
363 psi @Strain 100 % |
ISO 37 |
BASF Elastollan B 60 A ESD TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 2.50 MPa | 363 psi | 20; ISO 37 |
BASF Elastollan SP 806 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 2.50 MPa | 363 psi | 20; ISO 37 |
BASF Elastollan SP 9213 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | >= 2.50 MPa | >= 363 psi | perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r.. |
|||
Tensile Strength | 2.50 MPa @Strain 100 % |
363 psi @Strain 100 % |
ISO 37 |
BASF Elastollan C 70 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 2.50 MPa @Strain 100 % |
363 psi @Strain 100 % |
ISO 37 |
BASF Elastollan S 60 AWH TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 2.50 MPa @Strain 100 % |
363 psi @Strain 100 % |
ISO 37 |
BASF Elastollan B 60 A WHA TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |