Polymer Property : Tensile Strength = 363 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 2.50 MPa

@Strain 200 %
363 psi

@Strain 200 %
ISO 527
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound
PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri..
Tensile Strength 2.50 MPa
363 psi
Shin-Etsu Silicones KE-3479 Silicone, RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 2.50 MPa
363 psi
Shin-Etsu Silicones KE-347T Silicone, RTV Coating
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 2.50 MPa
363 psi
Shin-Etsu Silicones KE-3490 Silicone, RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 2.50 MPa
363 psi
Shin-Etsu Silicones KE-3490 Silicone, RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 2.50 MPa
363 psi
Shin-Etsu Silicones KE-3494 Silicone, RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 2.50 MPa

@Strain 20.0 %
363 psi

@Strain 20.0 %
ISO 37
BASF Elastollan 1185 A W TPUR
Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi..
Tensile Strength 2.50 MPa

@Strain 100 %
363 psi

@Strain 100 %
ISO 37
BASF Elastollan B 60 A ESD TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..
Tensile Strength 2.50 MPa
363 psi
20; ISO 37
BASF Elastollan SP 806 TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Tensile Strength 2.50 MPa
363 psi
20; ISO 37
BASF Elastollan SP 9213 TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Tensile Strength >= 2.50 MPa
>= 363 psi
perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..
Tensile Strength 2.50 MPa

@Strain 100 %
363 psi

@Strain 100 %
ISO 37
BASF Elastollan C 70 A HPM TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c..
Tensile Strength 2.50 MPa

@Strain 100 %
363 psi

@Strain 100 %
ISO 37
BASF Elastollan S 60 AWH TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tensile Strength 2.50 MPa

@Strain 100 %
363 psi

@Strain 100 %
ISO 37
BASF Elastollan B 60 A WHA TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..