Polymer Property : Tensile Strength = 17.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 17.7 MPa
2570 psi
Optimum; With provided formulation; ASTM D638
PolyOne Geon™ 120 Series 124A Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 124A is low molecular weight resin providing lower gelation and faster fusion characteristics. It provideds good chemical foamability for producing medium to high density foams. It gives good..
Tensile Strength >= 17.7 MPa
>= 2560 psi
ASTM D 638
Karina 85/201-DA-IS-SI-AT Clear PVC Compound
Non toxic PVC compound, free of phthalate plasticizers, recommended for stretch films for food contact use.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 17.7 MPa
>= 2560 psi
NBR NM-IEC 60811-1-1
Karina 905-32/170-CY-AC Orange PVC Compound
Weather resistant and flame retardant PVC compound, class 70CInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 17.7 MPa
>= 2560 psi
ASTM D 638
Karina 970-DA-48/1-B-IS Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 17.7 MPa
>= 2560 psi
ASTM D 638
Karina BTR-72/201-D-IS-SI Clear PVC Compound
Heavy metal free and additiveted with PU PVC compound, recommended for calendering of oil and solvent resistant Sheet.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 17.7 MPa
>= 2560 psi
ASTM D 638
Karina E 85/201-DA-IS-SI-AT Clear Crystal PVC Compound
Non toxic PVC compound, free of phthalate plasticizers, recommended for stretch films for food contact use.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength 17.7 MPa
2560 psi
Taiwan Sheen Soon Sheenthane® A7090 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength 17.7 MPa
2560 psi
20 in/min; ASTM D638
Teknor Apex Sinvicomp SHE 5200 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex
Tensile Strength 17.7 MPa
2560 psi
20 in/min; ASTM D638
Teknor Apex Sinvicomp SHE 5800 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex
Tensile Strength >= 17.7 MPa
>= 2560 psi
ASTM D 638
Karina E 85/201-DA-IS-SI Clear PVC Compound
Non toxic PVC compound, free of phthalate plasticizers, recommended for stretch films for food contact use.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 17.7 MPa
>= 2560 psi
ASTM D 638
Karina 900D10/120-IS-PO White PVC Compound
PVC powder compound, recommended for covering metallic parts in fluidized bed.Information provided by Karina Indústria e Comércio de Plásticos Ltda.