Teknor Apex Sinvicomp SHE 5800 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name Sinvicomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinvicomp SHE 5800 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
ASTM D2240
Tensile Strength 17.7 MPa
2560 psi
20 in/min; ASTM D638
Elongation at Break 300 %
300 %
20 in/min; ASTM D638