Karina E 85/201-DA-IS-SI Clear PVC Compound

Category Polymer , Film , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 85/201-DA-IS-SI Clear PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non toxic PVC compound, free of phthalate plasticizers, recommended for stretch films for food contact use.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.22 - 1.28 g/cc
1.22 - 1.28 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 81 - 85

@Time 15.0 sec
81 - 85

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 17.7 MPa
>= 2560 psi
ASTM D 638
Elongation at Break >= 150 %
>= 150 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Films
Clarity OK
ME 03