Polymer Property : Tensile Strength = 16.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 16.6 MPa
2410 psi
Dry Heat Aging 392°F; 168 hr; ASTM D865
Seals Eastern 5794 Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..
Tensile Strength 16.6 MPa
2410 psi
Plasticizer conc. in vinyl film 50 phr; ASTM D638
BASF Palatinol® N Diisononyl Phthalate
Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl..