Material Notes:
Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl compounds provides good low temperature and low volatility performance. It has excellent rheological properties in plastisols and offers improved dry blend times. The mechanical properties of vinyl compounds plasticized with Palatinol N are comparable to products plasticized with other diisononyl phthalates. The unique nature of this ester results in lower volatility, improved processibility and better low temperature performance.Applications: The excellent resistance to water and outdoor exposure by vinyl plasticized with Palatinol N is an advantage in the manufacture of articles for the housing and construction markets. By virtue of its contribution to low viscosity and good viscosity stability, Palatinol N is suitable for plastisols including: spray coating, dipping, casting and slush molding.Information provided by BASF
Physical Properties Metric English Comments
Density 0.970 - 0.976 g/cc
0.0350 - 0.0353 lb/in³
ASTM D4052
Solubility of Water 0.0020 %
0.0020 %
Solubility in Water <= 1.0e-6 %
<= 1.0e-6 %
Viscosity 28 cP

@Temperature 40.0 °C
28 cP

@Temperature 104 °F
Absolute
79 cP

@Temperature 20.0 °C
79 cP

@Temperature 68.0 °F
Absolute
345 cP

@Temperature 0.000 °C
345 cP

@Temperature 32.0 °F
Absolute
Molecular Weight 418 g/mol
418 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore A 69

@Time 15.0 sec
69

@Time 0.00417 hour
Plasticizer conc. in vinyl film 70 phr; ASTM D 2240
82

@Time 15.0 sec
82

@Time 0.00417 hour
Plasticizer conc. in vinyl film 50 phr; ASTM D 2240
89

@Time 15.0 sec
89

@Time 0.00417 hour
Plasticizer conc. in vinyl film 40 phr; ASTM D 2240
Tensile Strength 13.0 MPa
1890 psi
Plasticizer conc. in vinyl film 70 phr; ASTM D638
16.6 MPa
2410 psi
Plasticizer conc. in vinyl film 50 phr; ASTM D638
17.8 MPa
2580 psi
Plasticizer conc. in vinyl film 40 phr; ASTM D638
Elongation at Break 280 %
280 %
Plasticizer conc. in vinyl film 40 phr; ASTM D638
310 %
310 %
Plasticizer conc. in vinyl film 50 phr; ASTM D638
350 %
350 %
Plasticizer conc. in vinyl film 70 phr; ASTM D638
100% Modulus 0.0101 GPa
1.47 ksi
Plasticizer conc. in vinyl film 50 phr; ASTM D638
0.01410 GPa
2.045 ksi
Plasticizer conc. in vinyl film 40 phr; ASTM D638
0.0610 GPa
8.85 ksi
Plasticizer conc. in vinyl film 70 phr; ASTM D638
Torsional Stiffness 310 MPa

@Temperature -9.00 °C
45000 psi

@Temperature 15.8 °F
Plasticizer conc. in vinyl film 40 phr; ASTM D1043
310 MPa

@Temperature -22.0 °C
45000 psi

@Temperature -7.60 °F
Plasticizer conc. in vinyl film 50 phr; ASTM D1043
310 MPa

@Temperature -38.0 °C
45000 psi

@Temperature -36.4 °F
Plasticizer conc. in vinyl film 70 phr; ASTM D1043
Thermal Properties Metric English Comments
CTE, linear 700 µm/m-°C
389 µin/in-°F
Boiling Point 252 °C

@Pressure 600000 MPa
486 °F

@Pressure 8.70e+7 psi
Pour Point -49.0 °C
-56.2 °F
Brittleness Temperature -42.0 °C
-43.6 °F
Plasticizer conc. in vinyl film 70 phr; ASTM D746
-31.0 °C
-23.8 °F
Plasticizer conc. in vinyl film 50 phr; ASTM D746
-23.0 °C
-9.40 °F
Plasticizer conc. in vinyl film 40 phr; ASTM D746
Flash Point 240 °C
464 °F
Optical Properties Metric English Comments
Refractive Index 1.486
1.486
Chemical Properties Metric English Comments
Total Acid Number <= 0.070
<= 0.070
[mg KOH/g]; ASTM D1045
Processing Properties Metric English Comments
Moisture Content 0.10 %
0.10 %
ASTM E203
Descriptive Properties Value Comments
Color <25
APAH, ASTM D5386
Composition Ester content
>99.6%, ASTM D3465
Copyright © lookpolymers.com All Rights Reserved