Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 15.9 MPa | 2310 psi | ASTM D638 |
S&E Specialty Polymers G-2194 Application: Clear, UV resistant, extrusion compound.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 15.9 MPa | 2310 psi | ASTM D412 |
S&E Specialty Polymers TufFlex™ GTPE-9070J-34 TPE Compound Application: A 105°C rated, UV resistant, matte finish, TPE alloy jacketing compound for FT4 and riser applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 15.9 MPa | 2310 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ G-2194 Clear PVC Compound Application: Clear, UV resistant extrusion grade compound.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 15.9 MPa | 2310 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-3210 PVC Compound Application: 105°C insulating and jacketing material designed to meet UL 62 for SPT-1 and AWM. UL recognized for QMTT2 TW, THW.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 15.9 MPa @Strain 100 % |
2310 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B6DT0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 15.9 MPa @Strain 100 % |
2310 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B6DB1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 15.9 MPa @Strain 100 % |
2310 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible G92B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 15.9 MPa | 2310 psi | |
Lucite International Elvacite ® 2016 Acrylic Resin Elvacite® 2016 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. Elvacite® 2016 is useful in clear, translucent or pigmented metal lacquers. It is a fast dissolvi.. |
|||
Tensile Strength | 15.9 MPa | 2310 psi | |
Lucite International Elvacite ® 2697 Acrylic Resin Elvacite® 2697 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. Elvacite® 2697 is useful in clear, translucent or pigmented metal lacquers. It is a fast dissolvi.. |
|||
Tensile Strength | 15.9 MPa | 2300 psi | ASTM D638 |
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri.. |
|||
Tensile Strength | 15.9 MPa | 2300 psi | ASTM D412 |
Saint-Gobain Tygon® S3™ Silver Antimicrobial Tubing Plasticizer-free inner boreFormulated with a silver based compound on I.D. surfaceO.D. surface can also be formulated with a silver based compoundReduces formulation of biofilm and mildewInhibits gr.. |
|||
Tensile Strength | 15.9 MPa | 2300 psi | |
AlphaGary PVC GM 8015-M Natural LCF Polyvinyl Chloride Thermoplastic A lead / cadmium free, 105°C, UL-94 V-O rated, electrical grade molding compound |
|||
Tensile Strength | 15.9 MPa | 2300 psi | |
AlphaGary Garaflex™ E 4780-A5 LCF Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable105°C rated low temperature SEO insulation compound |
|||
Tensile Strength | 15.9 MPa | 2300 psi | |
AlphaGary GW 3040 LT LCF Flame Retardant Polyvinyl Chloride 90°C rated jacket compound for riser applications with improved low temperature performance |
|||
Tensile Strength | 15.9 MPa | 2300 psi | |
AlphaGary Smokeguard™ LS III 1021 UV FG Low Smoke Polyvinyl Chloride 80°C Rated Indoor/Outdoor Cable |
|||
Tensile Strength | 15.9 MPa @Strain 100 % |
2310 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R351AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |