Lucite International Elvacite ® 2016 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 2016 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvacite® 2016 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. Elvacite® 2016 is useful in clear, translucent or pigmented metal lacquers. It is a fast dissolving, low viscosity resin for lacquer and toner use.Information provided by Lucite International
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
Particle Size 170 - 265 µm
170 - 265 µm
Viscosity Measurement 0.23 - 0.255
0.23 - 0.255
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 60000 g/mol
60000 g/mol
Mechanical Properties Metric English Comments
Hardness, Knoop 8.0
8.0
Tukon Hardness
Tensile Strength 15.9 MPa
2310 psi
Elongation at Break 2.0 %
2.0 %
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 59.0 °C
138 °F
Chemical Properties Metric English Comments
Total Acid Number 3.5
3.5
Processing Properties Metric English Comments
Moisture Content 0.50 %
0.50 %
Users viewing this material also viewed the following: