Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 92.0 MPa | 13300 psi | DIN 53455 |
Isoflon PEEK Polyetheretherketone Materials with strong mechanical and electrical performances under high temperatures.Information provided by Isoflon. |
|||
Tensile Strength | 92.0 MPa | 13300 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (.. |
|||
Tensile Strength | 92.0 MPa | 13300 psi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Tensile Strength | 91.7 MPa | 13300 psi | ASTM D638 |
Ensinger Tecapeek® XP-119G Compression Molded PEEK Compound, 10% Carbon Fiber with 5% Graphite Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Strength | 92.0 MPa | 13300 psi | DIN 53 455 |
Hippe PEEK Polyetheretherketone PEEK is a crystalline, easily machinable thermoplastic which is characterized by high tensile and constant good electrical properties between 0°-220°C, as well as due to favorable tribological beh.. |
|||
Tensile Strength | 92.0 MPa | 13300 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (5 mi.. |