Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 91.7 MPa | 13300 psi | ASTM D638 |
Ensinger Tecapeek® XP-119G Compression Molded PEEK Compound, 10% Carbon Fiber with 5% Graphite Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |