Polymer Property : Tensile Strength = 124 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 124 MPa
18000 psi
Poco Graphite SUPERSiC® Si Silicon Carbide
The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for..
Tensile Strength 124 MPa
18000 psi
ASTM D638
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet)
Tensile Strength >= 124 MPa
>= 18000 psi
H.C. Starck Grain Stabilized Niobium (GSNb)
GSNb is a patent pending single-phase micro-alloy that has a grain size of approximately 2 ASTM numbers finer than standard commercial grade niobium.Applications: Grain Stabilized Niobium (GSNb) is..
Tensile Strength 124 MPa
18000 psi
ASTM D638
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good..
Tensile Strength 124 MPa
18000 psi
ASTM D638
Solvay Specialty Polymers Ryton® XE4050BL Polyphenylene Sulfide Alloy (PPS Alloy), GlassMineral Filled
Ryton® XE4050BL glass fiber and mineral filled polyphenylene sulfide alloy compound provides high ductility and impact strength along with good thermal stability.Features: Ductile; Good Thermal S..
Tensile Strength 124 MPa
18000 psi
5 mm/min; ISO 527-1
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber
SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme..
Tensile Strength 124 MPa

@Temperature 23.0 °C
18000 psi

@Temperature 73.4 °F
EN ISO 527
Ensinger TECASINT 4011 Polyimide, Yellow (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Tensile Strength 124 MPa
18000 psi
ASTM D638
E-Polymers SEPAZ® V220A 20% Glass Fiber Reinforced PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..
Tensile Strength 124 MPa
18000 psi
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air..
Tensile Strength 124 MPa
18000 psi
ASTM D638
Techmer ES HiFill FR® PA6 GF25 FR 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Flame RetardantFeatures: Flame Retardant UL File Number: E157318Processing Met..