Polymer Property : Tensile Strength = 117.2 MPa
Polymer Property :
Tensile Strength =
117.2 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength
117.2
MPa
17000
psi
ASTM D 638
MRC Polymers MAXNITEâ„¢ 550 GF30 PET, 30% Glass Mineral Reinforced
Information provided by MRC Polymers Inc.