Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.00 MPa | 1020 psi | ISO 37 |
Multibase TPSiV® 4200-50A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data) Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig.. |
|||
Tensile Strength | 7.03 MPa | 1020 psi | Silicone Property; ASTM D412 |
Arlon A4020-C004FR 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 15% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film FAR 25.853 Recognition: Product is des.. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ FFSL 7061 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ FFSL 7071 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ FSL 7661 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ LIM 6041 Liquid Silicone Rubber - Healthcare Radio Opaque (X-Ray Detectability) LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ LIM 6071 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ LIM 8040 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2080 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2680FC High Productivity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2725/40 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3696/20 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3786/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | Flatwise |
Henkel Hysol EA 9658 Film Adhesive High temperature and high durability film adhesive designed for high toughness and high temperature performanceApplications: Composite Bonding Metal and Honeycomb Bonding |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 4080 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 7060 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 7.00 MPa @Strain 100 % |
1020 psi @Strain 100 % |
ISO 37 |
BASF Elastollan 1185 A M TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 7.00 MPa @Strain 100 % |
1020 psi @Strain 100 % |
ISO 37 |
BASF Elastollan B 90 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | ASTM D 638 |
API Megol AM DP2217/90PBT SEBS Adhesion Modified Overmolding for Polyesters Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tensile Strength | 7.00 MPa | 1020 psi | ASTM D 638 |
API Megol AM T A SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tensile Strength | 7.00 MPa @Strain 100 % |
1020 psi @Strain 100 % |
ISO 37 |
BASF Elastollan 1185 A WM TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |