Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - Cl (Chloride) | <= 10 ppm | <= 10 ppm | Leachable |
GrafTech GRAFOIL® GHC Standard Internal Combustion Laminate GRAFOIL® Grade GHC is a laminate made from Grade GTC flexible graphite. Laminate Construction: GRAFOIL® Grade GTC ? Micro-thin, phenolic-based adhesive ? GRAFOIL® Grade GTC |
|||
Ionic Impurities - Cl (Chloride) | <= 10 ppm | <= 10 ppm | Leachable |
GrafTech GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTA premium flexible graphite is a non-inhibited grade developed for use in nuclear or semiconductor applications. It is certified to meet the most rigorous purity specifications of the .. |
|||
Ionic Impurities - Cl (Chloride) | 10 ppm | 10 ppm | Leachable |
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall.. |
|||
Ionic Impurities - Cl (Chloride) | <= 10 ppm | <= 10 ppm | Leachable |
GrafTech GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material GRAFOIL® GTC flexible graphite sheet is a gasketing material containing no binders or fillers, which will seal a wide variety of liquids and gases over an extremely large temperature range. GTC c.. |
|||
Ionic Impurities - Cl (Chloride) | <= 10 ppm | <= 10 ppm | Leachable |
GrafTech GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material GRAFOIL® GTJ premium flexible graphite is an oxidation/corrosion inhibited grade developed for use in nuclear and high temp, high purity applications. It is certified to meet the most rigorous pu.. |
|||
Ionic Impurities - Cl (Chloride) | 10 ppm | 10 ppm | Leachable |
GrafTech GRAFOIL® GTX Standard Fluid Sealing Graphite, Single Layer Material GRAFOIL® GTX flexible graphite sheet is inhibited for high oxidation/corrosion resistance that can be used for most fluid sealing and industrial applications. Grade GTX contains an inorganic, non.. |
|||
Ionic Impurities - Cl (Chloride) | 10 ppm | 10 ppm | Leachable |
GrafTech GRAFOIL® SUPER GTO® Standard Internal Combustion Single Layer Gasketing Material GRAFOIL® SUPER GTO® flexible graphite sheet is a gasketing material containing no binders, which will seal a wide variety of liquids and gases over an extremely large temperature range (-240Â.. |
|||
Ionic Impurities - Cl (Chloride) | <= 10 ppm | <= 10 ppm | |
Solvay Sulfuric Acid 93% Water White Grade Description Water White Sulfuric Acid is a clear, colorless oily-looking liquid. It is very corrosive.Formula: H2SO4 (in aqueous solution)Nomenclature: Sulfuric Acid, Oil of VitriolCAS: 7664-93-9CAS.. |
|||
Ionic Impurities - Cl (Chloride) | <= 10 ppm | <= 10 ppm | |
Solvay Sulfuric Acid Electrolyte Grade Description: Sulfuric Acid electrolyte grade is colorless, clear and non-fuming with no visible sediment. It is very corrosive. The 93.2% strength solution complies with the Federal Specification O-.. |
|||
Ionic Impurities - Cl (Chloride) | <= 10 ppm | <= 10 ppm | |
Epoxy Technology EPO-TEK® ED1021 Epoxy Preliminary Product Information SheetMaterial Description: A single component, silver-filled epoxy designed for low power semiconductor LED die attach applications. Unique features include its abil.. |
|||
Ionic Impurities - Cl (Chloride) | <= 10 ppm | <= 10 ppm | |
Epoxy Technology EPO-TEK® EK1000 Epoxy Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding .. |
|||
Ionic Impurities - Cl (Chloride) | <= 10 ppm | <= 10 ppm | |
Epoxy Technology EPO-TEK® EK2000 Epoxy Preliminary Product Information SheetMaterial Description: A two component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance .. |