Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - Na (Sodium) | 3.0 ppm | 3.0 ppm | |
Epoxy Technology EPO-TEK® ED1021 Epoxy Preliminary Product Information SheetMaterial Description: A single component, silver-filled epoxy designed for low power semiconductor LED die attach applications. Unique features include its abil.. |