Chemical Properties Metric English Comments
Ionic Impurities - Na (Sodium) 3.0 ppm
3.0 ppm
Epoxy Technology EPO-TEK® ED1021 Epoxy
Preliminary Product Information SheetMaterial Description: A single component, silver-filled epoxy designed for low power semiconductor LED die attach applications. Unique features include its abil..