Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0084 cm/cm @Time 86400 sec |
0.0084 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX DX11003 PC (Europe-Africa-Middle East) LNP FARADEX DX11003 is a compound based on Polycarbonate resin potentially suitable to meet high frequency electromagnetic absorption requirments. The compound is also an excellent candidate for man.. |
|||
Linear Mold Shrinkage, Flow | 0.0084 cm/cm @Time 86400 sec |
0.0084 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0084 cm/cm @Time 86400 sec |
0.0084 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRILOY D2000P PC LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing, Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0084 cm/cm @Time 86400 sec |
0.0084 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRILOY D2000P PC (Asia Pacific) LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing. |
|||
Linear Mold Shrinkage, Flow | 0.0084 cm/cm @Time 86400 sec |
0.0084 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0084 cm/cm @Time 86400 sec |
0.0084 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Asia Pacific) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0084 cm/cm @Time 86400 sec |
0.0084 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Europe-Africa-Middle East) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |