Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0064 cm/cm

@Time 86400 sec
0.0064 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC
LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible.
Linear Mold Shrinkage, Flow 0.0064 cm/cm

@Time 86400 sec
0.0064 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific)
LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
Linear Mold Shrinkage, Flow 0.0064 cm/cm

@Time 86400 sec
0.0064 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66
LNP* LUBRICOMP* RFL33 is a compound based on Nylon 66 resin containing 15% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Flow 0.0064 cm/cm

@Time 86400 sec
0.0064 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Asia Pacific)
LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0064 cm/cm

@Time 86400 sec
0.0064 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DX05499 PC
LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Linear Mold Shrinkage, Flow 0.0064 cm/cm

@Time 86400 sec
0.0064 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DX05499 PC (Asia Pacific)
LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.0064 cm/cm

@Time 86400 sec
0.0064 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU
LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing 20% Glass Fiber.
Linear Mold Shrinkage, Flow 0.0064 cm/cm

@Time 86400 sec
0.0064 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK
LNP* THERMOCOMP* LF005 is a compound based on Polyetheretherketone resin containing 25% Glass Fiber.
Linear Mold Shrinkage, Flow 0.0064 cm/cm

@Time 86400 sec
0.0064 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK (Asia Pacific)
LNP* Thermocomp* LF005 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Linear Mold Shrinkage, Flow 0.0064 cm/cm

@Time 86400 sec
0.0064 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp TH0450D
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
Linear Mold Shrinkage, Flow 0.0064 cm/cm

@Time 86400 sec
0.0064 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific)
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
Linear Mold Shrinkage, Flow 0.0064 cm/cm

@Time 86400 sec
0.0064 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Asia Pacific)
LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber.