Polymer Property : Linear Mold Shrinkage, Flow = 0.00090 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00040 - 0.00090 cm/cm

@Time 86400 sec
0.00040 - 0.00090 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE004 PC
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.00090 cm/cm

@Time 86400 sec
0.00040 - 0.00090 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific)
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00070 - 0.00090 cm/cm

@Time 86400 sec
0.00070 - 0.00090 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive.