Polymer Property : Linear Mold Shrinkage, Flow = 0.00040 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear
LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear
LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE003 PC (Asia Pacific)
LNP STAT-KON* DE003 is a compound based on Polycarbonate resin containing Carbon Fiber.
Linear Mold Shrinkage, Flow 0.00040 - 0.0013 cm/cm

@Time 86400 sec
0.00040 - 0.0013 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE003 PC (Asia Pacific)
LNP STAT-KON* DE003 is a compound based on Polycarbonate resin containing Carbon Fiber.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE003ER PC
LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.0013 cm/cm

@Time 86400 sec
0.00040 - 0.0013 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE003ER PC
LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE003P PC (Asia Pacific)
LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.0013 cm/cm

@Time 86400 sec
0.00040 - 0.0013 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE003P PC (Asia Pacific)
LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.00090 cm/cm

@Time 86400 sec
0.00040 - 0.00090 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE004 PC
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE004 PC
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.00090 cm/cm

@Time 86400 sec
0.00040 - 0.00090 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific)
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific)
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.0013 cm/cm

@Time 86400 sec
0.00040 - 0.0013 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC (Asia Pacific)
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Flow 0.00040 - 0.0013 cm/cm

@Time 86400 sec
0.00040 - 0.0013 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC (Asia Pacific)
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE003ER PC (Asia Pacific)
LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Flow 0.00040 - 0.0013 cm/cm

@Time 86400 sec
0.00040 - 0.0013 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE003ER PC (Asia Pacific)
LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE003P PC
LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Exceptional Processing.
Linear Mold Shrinkage, Flow 0.00040 - 0.0013 cm/cm

@Time 86400 sec
0.00040 - 0.0013 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE003P PC
LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Exceptional Processing.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE006ER PC
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.0013 cm/cm

@Time 86400 sec
0.00040 - 0.0013 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE006ER PC
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE006ER PC (Asia Pacific)
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Flow 0.00040 - 0.0013 cm/cm

@Time 86400 sec
0.00040 - 0.0013 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE006ER PC (Asia Pacific)
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.