Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.00373 bar @Temperature 120 °C |
2.80 torr @Temperature 248 °F |
AboCure |
Abatron AboCast/AboCure 8109-1 High melting point.Processing: 100/30 pbw; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).Applications: Heavy duty castin.. |
|||
Vapor Pressure | 0.00373 bar @Temperature 120 °C |
2.80 torr @Temperature 248 °F |
AboCure |
Abatron AboCast/AboCure 8109-2 High melting point. Filled version.Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°.. |