Physical Properties Metric English Comments
Vapor Pressure 0.00373 bar

@Temperature 120 °C
2.80 torr

@Temperature 248 °F
AboCure
Abatron AboCast/AboCure 8109-1
High melting point.Processing: 100/30 pbw; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).Applications: Heavy duty castin..
Vapor Pressure 0.00373 bar

@Temperature 120 °C
2.80 torr

@Temperature 248 °F
AboCure
Abatron AboCast/AboCure 8109-2
High melting point. Filled version.Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°..