Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vapor Pressure = 2.00 torr Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.00267 bar

@Temperature 1800 °C
2.00 torr

@Temperature 3270 °F
Plansee Chromium, Cr; Sintered
Characteristics:High corrosion resistanceHigh wear resistanceBeautiful opticsLower melting point than other refractory metalsVery high vapor pressureLower density than other refractory metalsPossess..
Vapor Pressure 0.00267 bar

@Temperature 120 °C
2.00 torr

@Temperature 248 °F
AboCure
Abatron AboCast/AboCure 8109-7
Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure...
Copyright © lookpolymers.com All Rights Reserved