Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plansee Chromium, Cr; Sintered

Category Metal , Nonferrous Metal , Pure Element
Manufacturer Plansee SE
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plansee Chromium, Cr; Sintered.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics:High corrosion resistanceHigh wear resistanceBeautiful opticsLower melting point than other refractory metalsVery high vapor pressureLower density than other refractory metalsPossesses lower modulus of elasticity than molybdenum and tungstenApplications:Wear-resistant coatingComponent parts in high temperature fuel cellsDecorative coating for appliances and jewelryInformation provided by Plansee.
Physical Properties Metric English Comments
Specific Gravity 7.15 g/cc
7.15 g/cc
a Lattice Constant 2.8847 Å
2.8847 Å
body-centered cubic
Vapor Pressure 0.00267 bar

@Temperature 1800 °C
2.00 torr

@Temperature 3270 °F
0.07161 bar

@Temperature 2200 °C
53.71 torr

@Temperature 3990 °F
Mechanical Properties Metric English Comments
Hardness, Vickers 180 - 250
180 - 250
Modulus of Elasticity 294 GPa
42600 ksi
Poissons Ratio 0.21
0.21
Shear Modulus 121 GPa
17500 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 6.20 µm/m-°C
3.44 µin/in-°F
Specific Heat Capacity 0.450 J/g-°C
0.108 BTU/lb-°F
Thermal Conductivity 93.7 W/m-K
650 BTU-in/hr-ft²-°F
Melting Point 1900 °C
3450 °F
Boiling Point 2672 °C
4842 °F
Chemical Properties Metric English Comments
Atomic Mass 51.996
51.996
Atomic Number 24
24
Atomic Volume 1.2e-029
1.2e-029
m^3
Users viewing this material also viewed the following: