Physical Properties Metric English Comments
Vapor Pressure 0.133 bar

@Temperature 60.0 °C
100 torr

@Temperature 140 °F
Solvay Specialty Polymers Galden® SV110 PFPE Solvent
Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature..
Vapor Pressure 0.133 bar

@Temperature 9.00 °C
100 torr

@Temperature 48.2 °F
Solvay Specialty Polymers Galden® SV55 PFPE Solvent
Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature..
Vapor Pressure 0.133 bar

@Temperature 32.0 °C
100 torr

@Temperature 89.6 °F
Solvay Specialty Polymers Galden® SV80 PFPE Solvent
Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature..